Meaning
Irreversible chemical breakdown of polymer chains caused by excessive heat or prolonged residence time during processing alters the mechanical and physical properties of the plastic. This degradation occurs when polyolefin thermal degradation breaks the covalent bonds of the backbone, leading to chain scission or crosslinking depending on the specific resin. The resulting reduction in molecular weight diminishes both impact strength and long-term durability.
Molecular Breakdown
Chain scission dominates in polypropylene, causing a substantial increase in melt flow rate and a loss of structural integrity. In contrast, polyethylene subjected to polyolefin thermal degradation tends to crosslink, which increases viscosity and creates gel particles that ruin film quality. These chemical changes are initiated by free radicals that form when the polymer is exposed to heat and oxygen in the extruder barrel.
Processing Defect
Unstable melt flow and varying viscosity lead to severe molding issues such as flash or short shots. When polyolefin thermal degradation occurs, the gas generated by the breaking polymer chains can cause voids and silver streaks on the molded surfaces. These defects not only ruin the appearance of the parts but also indicate that the mechanical properties have been compromised.
Stability Management
Preventing this degradation requires careful control of barrel temperatures and the addition of primary and secondary antioxidants. Processors must minimize residence time in the barrel to prevent the polymer from overheating during interruptions. Properly managed melt temperatures and stabilizing additives ensure that the resin can be processed, and even recycled as regrind, without suffering significant loss in mechanical performance.
This protective strategy is essential for maintaining the tough elastomeric phase in modified polymers, preventing brittle failures in demanding structural applications.