Meaning
Non-destructive high-resolution X-ray computed tomography provides three-dimensional spatial tensor mapping of discrete reinforcement fibers, structural inclusions, or porous voids within polymer parts. The micro-ct orientation measurement establishes quantitative orientation tensors, vector distributions, and skin-core structural gradients across complex geometries without inducing mechanical damage through physical sectioning. It governs structural durability analysis, anisotropic structural warpage predictions and process verification for fiber-reinforced technical plastics, stopping where resin and filler exhibit near-identical X-ray attenuation coefficients, or where component wall dimensions surpass the penetration capability of the laboratory tube voltage.
Scan Reconstruction
Radiographic projection series are captured across continuous 360-degree specimen rotations, allowing numerical algorithms to generate volumetric voxel reconstructions of the sample. In micro-ct orientation routines, differential attenuation between the surrounding polymer matrix and higher-density glass fibers produces clear greyscale contrast. Edge-detection software determines the directional axis of every resolved fiber path, calculating the second-order orientation tensor components known as A11, A22, and A33.
Spatial resolution down to sub-micron scales is required to isolate individual filament boundaries in thirty-percent glass-filled polyamide or polybutylene terephthalate. Insufficient spatial resolution merges adjoining fibers, distorting directional vector calculations.
Flow Distribution
Mould injection kinematics establish distinct structural divisions across the component thickness, dividing walls into aligned frozen skins, disordered intermediate transition shells and transverse core layers. Applying micro-ct orientation protocols shows that fountain flow aligns fibers strictly parallel to the melt direction along mold surfaces, while expanding central flow paths force fibers perpendicular to primary cavity flow. Weld lines disrupt regular fiber continuity, leaving narrow zones with out-of-plane fiber tilting or missing reinforcement.
Verifying these local orientation tensors against finite element injection simulations reveals fill deviations that cause unpredicted perimeter warpage. Reworking cavity gate designs resolves asymmetric tensor balances before tooling steel undergoes hardening.
Defect Correlation
Structural stiffness calculations fail if isotropic modulus assumptions replace real three-dimensional fiber alignments. Tensile bar coupons sourced from production moldings yield anisotropic modulus variations exceeding forty percent between perpendicular cutting axes. High-resolution micro-ct orientation scans identify fiber attrition caused by excessive shear inside plasticizing barrels or narrow hot runner tips.
Fiber length degradation reduces load transfer efficiency regardless of directional alignment. Assessing internal structures through volumetric imaging prevents premature mechanical failure under dynamic cyclic stress.