Meaning
Standardized mechanical test procedures define the notched Charpy impact resistance of rigid plastics under edgewise pendular strike conditions. The specific designation iso 179-1/1ea prescribes an edgewise blow using test specimen Type 1, notch Type A, evaluated under non-instrumented pendular energy release. The metric determines how effectively a polymer material absorbs sudden kinetic impact when a sharp notch concentrate stresses at a defined point along the bar.
The standard applies to rigid thermoplastic and thermoset moulding compounds, but stops applying to cellular polymers, flexible elastomers, and materials that do not fracture or show measurable energy absorption under pendulum limits.
Specimen Configuration
Rectangular test bars measuring eighty millimeters in length, ten millimeters in width, and four millimeters in thickness serve as the standardized test specimen. Testing under iso 179-1/1ea dictates an A-notch, which features a forty-five-degree included angle terminating in a tip radius of zero point two five millimeters with an eight-millimeter remaining width beneath the notch. Machining or injection moulding this radius requires tight dimensional tolerances, as minor variations in the notch root radius dramatically distort measured energy absorption values.
Striking the bar edgewise directs the kinetic hammer blow against the narrow face opposite the notched face.
Datasheet Divergence
Raw material datasheets publish impact values obtained from virgin test bars conditioned at standard temperature and humidity. Measured iso 179-1/1ea energy levels on neat virgin polyamides or polycarbonates rarely match the actual performance of complex injection moulded parts, because gate locations, knit lines, and wall thickness gradients create local stress fields absent in test specimens. Incorporating post-industrial regrind or recycled resin reduces notched impact strength through molecular chain degradation, even when standard tensile modulus values remain unchanged.
Processors conducting incoming quality checks compare batch notch values against supplier limits to identify degraded or contaminated resin lots.
Failure Mode Determination
Fracture surfaces generated during pendular strikes reveal whether a resin exhibits brittle or ductile failure under sharp mechanical notches. Brittle breaks absorb minimal pendulum energy, registering single-digit kilojoules per square meter under iso 179-1/1ea, while tough resins yield hinged or incomplete breaks requiring high impact energy. Glass fiber reinforcement alters the failure dynamic by suppressing yielding, transforming ductile base polymers into rigid composites that fail through fiber pullout.
The recorded Charpy notch value defines the structural impact limit for moulded enclosures subjected to sudden external drops.