Meaning
Water content in raw or regrind polymer resins prior to drying governs the duration and thermal energy required to achieve a moldable state. The level of incoming pellet moisture varies widely depending on previous exposure to atmospheric humidity, storage conditions, and whether the resin is virgin or regrind. When this moisture level is exceptionally high, the drying system must run at peak load to bring the resin down to the required parts-per-million limit.
Measuring this value before starting a production run prevents the molding of wet material and secures the mechanical strength of the final product.
Drying Load
Desiccant beds must work harder when high incoming pellet moisture requires longer cycle times and higher temperatures. If the dryer cannot handle the moisture load, the resin will remain wet, leading to hydrolytic degradation during molding. Adjusting the drying cycle parameters based on pre-dried material status ensures that the material is fully prepared for processing.
Material Origin
Regrind material often contains higher moisture than virgin pellets due to exposure during previous molding runs or granulation. This means that blends with high regrind ratios require closer monitoring to achieve the same dryness. Proper storage of regrind minimizes the incoming pellet moisture variations.
Defect Prevention
Tracking the moisture levels before feeding the resin to the extruder prevents issues like surface splay and structural weakness. Since raw polymers are often shipped in non-airtight containers, incoming pellet moisture is a dynamic variable that must be managed through scheduled testing. Constant monitoring avoids the costly scraping of molded parts.