Meaning
Chemical resistance testing of moulded plastics often involves exposure to specific alcohols to evaluate their susceptibility to environmental stress cracking. The process of ethanol screening is a common test protocol used to measure how a polymer part performs when it comes into contact with sanitizers or solvents. This procedure evaluates the physical integrity of the moulded part under a combination of mechanical stress and chemical exposure.
It is particularly useful for medical and consumer housing parts that are disinfected frequently during their service life.
Test Protocol
Moulded test bars or finished parts are placed under a fixed bending strain using a curved fixture. During ethanol screening, the strained parts are exposed to ethanol solutions and monitored for the appearance of cracks or crazes. This test exposes molded-in stress that might otherwise remain hidden until the part is in service.
Mechanical Failure
Stress cracking occurs when the solvent penetrates the polymer structure and increases molecular mobility. In the case of ethanol screening, this absorption leads to microvoid formation and subsequent crack propagation under load. Amorphous polymers like polycarbonate are highly susceptible to this failure mode.
Processing Influence
Moulding conditions determine the residual stress levels in the finished part, which directly affects test survival. When the melt temperature is too low or the packing pressure is too high, the moulded parts fail ethanol screening rapidly due to high internal stresses. Moulders can improve test performance by raising the mould temperature to promote relaxation of the polymer chains during the cooling phase.
This adjustment reduces the molded-in stress and prevents the chemical from initiating cracks at the surface of the part, ensuring the final product meets the required durability standards.