Meaning
High-speed powder-metallurgical tool steel alloyed with tungsten, molybdenum and vanadium provides high abrasive wear resistance and compressive yield strength for demanding plastic conversion tooling. The DIN 1.3344 specification, equivalent to AISI M3 Class 2, governs a matrix featuring approximately 6 percent tungsten, 5 percent molybdenum and 3 percent vanadium carbides. Injection moulders select this grade for core pins, gate inserts and sliding shut-offs subject to high glass-fibre loading.
Corrosion resistance remains low compared to stainless tool grades, requiring controlled storage environments or physical vapour deposition coatings.
Carbide Structure
Powder metallurgical processing generates an isotropic carbide distribution free of the coarse segregation bands found in conventionally cast high-speed steels. Fine vanadium carbides pin grain boundaries during austenitisation, allowing achievable hardness values between 60 and 64 Rockwell C without sacrificing fracture toughness. The absence of stringer carbides prevents micro-chipping on delicate shut-off corners under clamp pressure.
High secondary hardening temperatures allow chemical vapour deposition treatments without matrix softening.
Abrasive Resistance
Engineering polymers containing forty to fifty percent chopped glass or mineral fillers induce rapid gate erosion during fill stages. Core components fabricated from din 1.3344 resist wall thinning and gate enlargement under repetitive high-velocity melt shear. Sub-gate orifices retain sharp shearing edges over millions of cycles, eliminating long stringy gate vestiges on finished parts.
Regrind materials containing foreign particulates or degraded polymer lumps cause less gouging damage across inserts hardened to this specification.
Thermal Response
Moderate thermal conductivity around 24 Watts per metre Kelvin requires strategic cooling line placement to avoid localized hot spots in deep core profiles. Dimensional stability across heat treatment cycles limits finish-grinding stock allowances, reducing tooling fabrication hours. Spark erosion procedures demand reduced spark energy passes to eliminate the brittle remelt layer prone to micro-cracking under injection pressure cycles.
DIN 1.3344 secures operational life across mould inserts where standard chromium steels wash out under filled resin flows.