Meaning
Volumetric contraction resulting from the tighter spatial packing of polymer chains during cooling and crystallisation marks the physical transition of thermoplastic melts into solid structures. A continuous density increase governs volumetric shrinkage rates and final part dimensions. Measurement occurs by comparing molten specific volume from pressure-volume-temperature curves against room-temperature displacement values.
The phenomenon applies exclusively to cooling transitions and stops once molecular chains reach vitrification or complete crystallisation.
Packing Phase
Holding pressure applied during injection moulding compensates for the volumetric loss that accompanies phase transformation. As molten resin cools, the density increase pulls material away from mould cavity walls unless the machine screw drives supplementary melt into the tool. Gate freeze ends this compensatory packing window abruptly.
Thick sections that experience delayed gate freeze develop internal voids or severe sink marks as continuing density increase contracts unpressurised internal resin pools.
Tool Dimensioning
Toolmakers cut cavity geometries larger than nominal part drawings to counter the density increase that develops between melt temperature and ambient factory conditions. Unfilled polyolefins undergo substantial density shifts during solid-state formation, requiring shrinkage steel allowances exceeding two percent. Mineral or glass reinforcements suppress bulk shrinkage by replacing contracting polymer volume with inert, dimensionally static particles.
Virgin resins track published density scales reliably across lots. Variable regrind fractions, however, introduce broken chain segments and prior thermal histories that alter packing behavior unpredictably. When regrind content fluctuates inside feed hoppers, the resulting erratic density increase distorts finished part tolerances and forces frequent holding pressure adjustments across production runs.
Crystallisation Influence
Amorphous resins demonstrate predictable, gradual volume reduction governed by thermal expansion coefficients alone. Semicrystalline polymers exhibit a sharp volumetric drop when disordered molecular chains fold into orderly crystalline lamellae, accelerating density increase across narrow temperature bands. Rapid tool quenching suppresses crystalline perfection, yielding parts with slightly lower final density and smaller shrinkage.
Conversely, high mould temperatures promote maximum crystal formation, driving larger density increase values that worsen differential shrinkage across varying wall thicknesses.