Chemical analysis of carboxyl end groups in polyesters measures the number of terminal acidic sites per unit mass of polymer. This metric, known as the CEG concentration, determines how susceptible a resin is to hydrolytic degradation during processing. A lower value indicates a more stable polymer that can withstand thermal stress without losing molecular weight.
Chemical Metric
Carboxyl concentrations are measured in milliequivalents per kilogram of polymer. In polyethylene terephthalate, a low CEG concentration is desirable because each acid group acts as a catalyst for chain breakdown. Processors measure this property before moulding to predict how the resin will perform under heat.
Hydrolytic Risk
Moisture in the extruder reacts with the ester linkages to accelerate polymer chain breakdown. When the CEG concentration is high, this hydrolysis reaction occurs much faster, leading to a sudden drop in melt viscosity. This chain breakdown produces shorter molecules that reduce the impact strength and tensile properties of the moulded part.
Melt Stability
Resin stability during extrusion depends directly on minimizing these terminal acid groups. Moulders must ensure that the starting CEG concentration is below thirty milliequivalents per kilogram for high-performance applications. Achieving this requires precise control of the polymerization reaction at the resin plant, as well as thorough desiccant drying before the polymer is heated in the extruder barrel.
A stable melt allows the processor to run the machine with consistent cycle times and minimal deviation in part dimensions, which is required for medical and automotive moulding operations.