Meaning
Chemical chain extenders bearing two carbodiimide functionalities react with active hydrogen atoms to arrest polyester degradation and restore molecular weight. Compounding operations introduce bis-carbodiimide into condensation polymers such as polybutylene terephthalate and polylactic acid to consume terminal carboxyl groups generated during melt processing. By capping these carboxylic acid ends, the additive terminates the autocatalytic hydrolysis pathway that otherwise cleaves polymer chains during service in humid environments.
The reaction ceases to provide stabilization once all carbodiimide moieties convert into stable acylurea bridges or when unreacted moisture levels overwhelm the initial stoichiometric concentration.
Polymer Stabilization
Hydrolytic degradation cleaves ester linkages into separate alcohol and carboxylic acid end groups. The free carboxylic acid acts as an internal catalyst, accelerating subsequent chain scission at elevated humidity. Adding bis-carbodiimide converts each terminal carboxyl group into an acylurea linkage, coupling two distinct polyester fragments into an extended polymer chain.
Melt viscosity climbs as this chain coupling proceeds, counteracting the rheological drop caused by thermal or moisture breakdown in the barrel. Overdosing the additive produces branched or lightly gelled networks, yielding unmelts and surface defects across injection moulded parts.
Dosage Calculation
Processors establish additive concentrations by measuring the carboxyl end group content of incoming virgin pellets or recycled flake. A baseline titration yields carboxyl concentrations in equivalents per ton, establishing the exact quantity of bis-carbodiimide needed to cap the acidic sites. Virgin polybutylene terephthalate typically carries a low carboxyl value, demanding light stabilizer loading between zero point two and zero point five percent by weight.
Reprocessed polyester scrap exhibits degraded chain ends, requiring heavier additions up to one point five percent to restore melt integrity. Excessive addition generates unreacted carbodiimide residues, which migrate toward the cavity surface and generate tool plate-out during continuous production.
Moulding Window
Decompression settings and barrel residency govern the consumption rate of reactive stabilizers in injection moulding. Barrel temperatures must supply sufficient thermal energy to activate carboxyl addition without crossing the thermal decomposition threshold of the carbodiimide structure. If residency extends beyond standard cycle allowances, the bis-carbodiimide reacts completely, leaving parts without residual additive reserves for environmental exposure.
Insufficient dwell time leaves the compounding reaction unfinished, leading to parts with uneven molecular weight and erratic ejection properties. Operating parameters must balance complete reaction against unnecessary thermal exposure to guarantee uniform tensile retention throughout the final product.