Meaning
Pendulum based measurement of the energy required to extend a tear in plastic film. astm d1922 calculates the force required to continue a rip through a specimen using a falling arm that loses momentum during the process. The resulting value describes how easily a package might continue to fail once an opening is initiated.
Propagation Energy
Mechanical resistance depends on the ability of the polymer to dissipate energy across a wide area. High energy absorption in astm d1922 implies that the material can withstand rough handling without total failure. When a film lacks this capacity, it often splits entirely upon the first point of contact with a sharp edge.
Directional Anisotropy
Polymer chains align along the direction of flow during the production of blown or cast film. This orientation causes the astm d1922 value to change depending on whether the tear is longitudinal or transverse. Machine direction values often appear lower because the tear travels between aligned chains.
Transverse results tend to be higher as the rip must break across the backbone of the molecules.
Property Balance
Blending low density and linear low density resins allows for the optimization of the tear strength. The astm d1922 result is checked against the stiffness of the material to ensure the bag remains functional. Higher density resins typically reduce tear resistance while increasing the barrier performance.
Moulders monitor this trade off to maintain part integrity at the lowest possible cost.