Meaning
Cyclical surface defect characterized by alternating bands of high and low gloss appears on large injection moulded parts. The presence of tiger striping is usually linked to flow instabilities at the melt front as it moves through the mold cavity. This defect is particularly common in polypropylene compounds used for automotive bumpers and interior panels.
Flow Instability
Movement of the polymer melt fluctuates between stick and slip conditions near the mold wall. When the melt front velocity reaches a certain threshold, the shell layer becomes unstable and creates the periodic pattern known as tiger striping. Flow oscillates.
This behavior is often driven by the viscoelastic properties of the resin and the geometry of the runner system.
Visual Impact
Rejection rates for painted or textured parts increase sharply when these surface marks are visible. Although tiger striping does not usually affect the structural integrity of the part, it is unacceptable for high end consumer products. The alternating bands are visible even through several layers of paint or primer.
Process Correction
Adjustments to the moulding parameters can often mitigate the severity of the surface defect. Increasing the melt temperature or the mold temperature helps by reducing the viscosity and smoothing out the flow, which prevents the rapid fluctuations in pressure that trigger the marking. Process stability improves when the injection speed is lowered.
If process changes fail, the resin supplier may adjust the rubber content or the molecular weight distribution of the polymer to improve flow stability.