Meaning
Fluid state achieved above specific temperature and pressure thresholds where liquid and gas phases merge into a single homogeneous medium. Supercritical carbon dioxide acts as a blowing agent during structural foam injection moulding. Processing equipment introduces this fluid directly into the polymer melt barrel under high pressure to dissolve the gas uniformly before the shot enters the mould cavity.
Dissolved gas lowers the melt viscosity of engineering thermoplastics and permits lower barrel temperatures during production runs.
Process Economics
Virgin resin economics benefit from reduced material density because the dissolved gas creates microcellular structures within moulded parts without adding heavy mass. Regrind economics require strict monitoring of melt flow indices because repeated thermal cycles alter how the polymer accepts gas saturation. Part specifications dictate allowable void fractions, whereas material specifications establish baseline melt mass flow rates before fluid injection begins.
Gas dosing units control mass flow rates relative to polymer throughput to maintain stable cell growth during expansion. Pressure drops across the nozzle trigger phase separation, nucleating millions of tiny bubbles simultaneously as the melt enters the cooler mould walls.
Dimensional Stability
Moulder settings determine final part tolerances by balancing mould temperature against gas dosage pressure. Tooling design must accommodate shrinkage variations caused by cell nucleation because underpacking leads to severe sink marks on thick wall sections. Part warp increases when injection speed fluctuates because uneven cooling freezes residual stresses into the skin layer.
Datasheet values for tensile strength apply to solid plaques, whereas moulded parts containing microcellular foam exhibit reduced stiffness along core sections. Process variables such as back pressure and screw rotation speed dictate cell density and average bubble diameter across the finished component.
Defect Formation
Surface swirl marks appear when melt temperature drops below the optimal window during injection into cold tools. Flash occurs along parting lines if injection pressure exceeds the clamping force during the expansion phase. Voids expand uncontrollably if mould cavity pressure drops too rapidly before the polymer skin solidifies completely.
Cost penalties mount when scrap rates rise due to surface blistering caused by excessive gas saturation in the melt stream. Precise calibration of injection profiles prevents structural collapse and ensures uniform weight reduction across production batches.