Meaning
Spatial variation in crystalline structure and molecular orientation between the surface and the interior of a moulded part arises from non-uniform cooling rates and shear flow during injection. The skin core morphological gradient is established as the hot polymer melt contacts the cold mould steel, creating distinct physical zones across the part thickness. This gradient determines the localized mechanical performance and dimensional stability of the finished component.
Cooling Phase
Polymer melt at the outer surface cools almost instantly upon contact with the cold steel walls, preventing the formation of large crystal structures. The center of the part remains hot for a longer duration, allowing the polymer chains to organize into a highly crystalline core. This difference in cooling rates creates a pronounced skin core morphological gradient across the part cross-section.
The thickness of each layer is determined by the mould temperature and the thermal conductivity of the polymer, which can be optimized to control the balance of stiffness and impact resistance.
Molecular Orientation
High shear stress during the filling phase stretches and aligns the polymer chains near the mould walls before they freeze in place. This shear-induced alignment contributes to the skin core morphological gradient by producing a highly oriented skin layer and a relatively unoriented core. The aligned chains in the skin layer provide high tensile strength in the direction of the melt flow.
Mechanical Impact
Unbalanced stresses within the finished part can lead to warpage and dimensional instability when the parts are ejected from the mould. Minimizing the skin core morphological gradient through optimized cooling rates and melt temperatures prevents these defects from occurring. A uniform cross-sectional structure ensures that the mechanical load is distributed evenly across the part.