Meaning
Concentration levels of absorbed solvents or plasticizers mark the transition where a polymer changes from a rigid, glassy state to a flexible, rubbery state at a given temperature. Reaching the plasticization threshold causes a sharp drop in the glass transition temperature of the resin, significantly altering its mechanical and thermal performance. In injection moulding, this transition can occur prematurely if the material absorbs too much moisture or if regrind containing high levels of processing aids is used.
Understanding this critical point helps moulders set correct drying times and process temperatures to avoid part deformation during ejection.
Transition Point
Free volume within the polymer matrix increases as the small molecules of the plasticizer insert themselves between the long polymer chains. When this free volume exceeds a critical limit, the chains gain the mobility required to slide past each other easily. This microscopic change corresponds to the plasticization threshold, which can be detected experimentally via dynamic mechanical analysis or differential scanning calorimetry.
Structural Response
Tensile strength and modulus of elasticity decrease rapidly once the plasticizer concentration surpasses this critical level. While this change is desirable in the manufacture of flexible films, it represents a catastrophic failure mode for structural parts that must support loads. Designers must ensure that the exposure of the polymer part to environmental chemicals does not drive it past this threshold during its service life.
Mechanical Failure
Drift in the mechanical properties of a moulded part can lead to warpage, cracking, or premature failure in the field. When the polymer exceeds its plasticization threshold, it becomes more susceptible to environmental stress cracking and creep. Regular testing of the raw resin and the finished parts ensures that the additive levels remain within the safe, glassy regime.