Meaning
Surface damage and material transfer between sliding metal surfaces occurs when high friction and localized welding tear away micro-junctions between moving parts. In injection moulding tooling, pin galling typically affects ejector pins and core pins that operate under high cycle speeds and elevated temperature. This friction-induced wear can lead to pin seizure, causing extensive downtime and damage to the mould steel.
Mechanical Failure
Insufficient lubrication or excessive side-loading of the ejector plate triggers the progressive degradation of the sliding metal surfaces. As the pin moves back and forth within the ejector bushing, the absence of a protective lubricant film allows direct metal-to-metal contact. The resulting frictional heat creates microscopic welds that rupture, leaving gouges that eventually jam the pin in place.
Friction Mitigation
Applying specialized high-temperature grease to the sliding surfaces is the standard method to prevent adhesive wear. Alternatively, using surface coatings like titanium nitride or diamond-like carbon provides a hard, low-friction barrier that resists damage.
Maintenance Schedule
Implementing scheduled cleaning and lubrication runs prevents the onset of adhesive damage before it compromises the production cycle. Toolroom technicians must regularly inspect the ejector system for the fine metallic dust that precedes severe scoring. Detecting these wear particles early allows for cleaning and re-coating before the mould incurs permanent structural damage.