Meaning
Strain-controlled axial fatigue testing specifies standard testing conditions to determine material response under low-cycle mechanical degradation. Test laboratories apply ISO 12106 to measure cyclic strain life and stress-strain hysteresis loops in tooling alloys used for injection moulding cores. The document defines strain measurement accuracy and waveform shapes required for uniaxial testing.
Its scope covers metallic materials subjected to constant-amplitude strain and excludes high-frequency acoustic fatigue regimes.
Tooling Fatigue
Injection mould cores experience cyclic thermal and mechanical loading during injection and packing steps. Following ISO 12106 procedures provides accurate cyclic stress-strain curves that reveal whether tool steel undergoes cyclic hardening or cyclic softening. Tool steel selection based on low-cycle fatigue data prevents premature thermal fatigue cracking in high-volume moulding operations.
Data Application
Datasheet elastic limits reflect static yield behavior rather than performance under repeated high-strain injection cycles. Standard testing per ISO 12106 evaluates plastic strain range and elastic strain range across thousands of reverse loading cycles. Tooling engineers use these fatigue parameters to design core pins capable of enduring pressure spikes during cavity filling.
Ignored plastic strain accumulation results in tool core deflection and wall thickness variation in moulded containers.
Method Limit
Axial testing methods described in the standard assume uniform strain distribution across the gauge section. Testing stops delivering valid material property data once macrocracking causes localized strain concentration within the specimen.