Meaning
Downward flow of a molten polymer under the force of gravity occurs most frequently during the extrusion of heavy wall pipes or large parisons. Managing gravitational sag is essential for maintaining wall thickness uniformity around the circumference of a horizontal extrudate. This phenomenon is driven by the low shear viscosity of the resin at processing temperatures.
Vertical Displacement
Molten material at the top of a profile tends to migrate toward the bottom before the cooling tank can solidify the part. Excess gravitational sag leads to a characteristic teardrop shape where the upper wall is thinner than the lower section. This vertical stretching is most pronounced in parisons with a high length to diameter ratio where the cooling time is extended.
Vacuum sizing and internal air pressure are used to counteract this movement during the initial cooling phase.
Viscosity Control
Resins with high zero shear viscosity are preferred for large profiles because they resist deformation over long periods. When gravitational sag is detected, processors may lower the melt temperature to increase the flow resistance of the polymer.
Wall Uniformity
Variations in cooling rates can exacerbate the uneven distribution of material caused by gravity. Precise calibration of the cooling bath prevents the temperature gradients that allow gravitational sag to continue deep into the solidification process.