Meaning
Geometrical defect occurs when the force required to push a part out of the mould exceeds the structural strength of the warm plastic. Ejection distortion typically appears as white stress marks or localized thinning in the part walls. It involves a failure of the mechanical interface between the ejector pins and the solidified polymer.
The problem vanishes when the part is cooled to a temperature where its modulus can resist the force of the pins.
Mechanical Resistance
Pin placement must distribute the force across the strongest sections of the part to prevent damage. If the ejection distortion happens near a thin rib, the concentrated pressure will punch through the material. Increasing the surface area of the pins reduces the localized pressure.
Smooth cavity finishes and draft angles lower the total force needed.
Temperature Variable
Melt temperature and cooling time are the primary factors that influence the risk of deformation. A high temperature at the moment of ejection means the material is still soft and prone to flow. When the ejection distortion is caught early, increasing the cooling time is the standard fix.
This change lengthens the cycle and increases the part cost.
Mould Maintenance
Contamination on the cavity surface or worn textures can increase the friction between the steel and the plastic. Regular cleaning prevents the buildup of waxes or additives that might make the part stick. Polishing the draw surfaces in the direction of ejection helps the part slide out.
A well maintained tool requires less force and produces fewer defects.