Meaning
Gravimetric force application establishes standardised mechanical stress on polymer melts inside capillary melt indexers by placing calibrated masses directly atop a piston assembly. This mass configuration enforces constant vertical force to measure the melt flow rate or melt volume rate of thermoplastic resins according to ISO 1133 and ASTM D1238. Standard test procedures prescribe discrete load levels ranging between 0.325 kg and 21.6 kg to accommodate different molecular weight profiles and viscosity classes.
Deadweight load scaling terminates its utility where non-linear shear rates demand variable piston speeds generated by electromechanical drives.
Testing Mechanism
Calibrated alloy weights seat onto the upper terminal of a hardened steel piston resting inside a heated barrel. Constant gravitational pull drives the piston downward, forcing molten resin through a standard tungsten carbide orifice. Operators alter the applied load based on resin type, moving from low masses for free-flowing grades to high masses for stiff extrusion materials.
High-viscosity polymers such as high molecular weight polyethylene require heavier masses to produce measurable extrudates within standardised cutting intervals.
Rheological Evaluation
Increasing the gravimetric load raises the shear stress applied to the polymer chains confined within the entrance of the capillary die. Measuring mass flow rates across multiple standard loads yields an index of pseudoplastic behaviour without employing dynamic capillary rheometry. Fractional melt flow resins exhibit substantial flow increases under elevated loads because chain alignment lowers apparent melt viscosity.
Resins exhibiting low sensitivity to mass increases possess narrower molecular weight distributions and lower shear responsiveness.
Moulding Translation
Datasheet values derived under low deadweight loads fail to capture the extreme shear conditions present inside an injection moulding runner or cavity gate. Injection pressures often exceed 100 MPa, whereas standard deadweight testing operates under mere fractions of a megapascal. Process engineers utilise load scaling ratios primarily for raw material incoming verification rather than tool fill simulation.
Variations in flow rates at identical load configurations signal batch-to-batch variations in base polymer molecular weight or regrind contamination.