Meaning
Localized micro-yielding in glassy polymers precedes macroscopic fracture by forming networks of fibrils and voids. Crazing mechanisms govern how plastics deform under tensile stresses below the yield point. These micro-cracks contain oriented polymer fibrils that span the gap between the bulk polymer walls, which provides some load-bearing capacity.
This phenomenon distinguishes crazing from true cracking, where no bridging material remains to hold the surfaces together.
Fibrillar Growth
Tensile stress causes localized cavitation in the polymer matrix, which forms tiny voids that grow and coalesce. The polymer chains between these voids then stretch and orient to form the load-bearing fibrils. This fibril structure remains stable until the stress exceeds the tensile strength of the oriented chains.
Once the fibrils break, the craze transforms into a true crack that can propagate rapidly to cause catastrophic brittle failure.
Stress Concentration
Structural defects and inorganic fillers act as initiation sites for craze formation by creating localized stress fields. The spacing and size of these defect sites dictate whether crazing spreads throughout the part or concentrates in a single region. Dispersing the stress over many small crazes absorbs more mechanical energy and increases the overall toughness of the plastic part.
Consequently, rubber-toughened polymers utilize localized crazing to prevent catastrophic brittle crack propagation.
Environmental Influence
Chemical agents accelerate craze initiation by lowering the surface energy of the polymer or plasticizing the chains. This environmental stress cracking occurs at load levels far below the dry mechanical limit. Proper resin selection prevents early failure in harsh chemical exposures.