Meaning
Chemical fragments generated during the thermal or hydrolytic degradation of polymers represent the breakdown products of larger macromolecular chains. These cleavage products often arise when resin is processed at temperatures exceeding its thermal stability limit during injection molding. Their presence indicates chain scission which degrades the mechanical strength of the molded component.
Degradation Mechanism
High shear forces and excessive melt temperatures within the extruder barrel cause the covalent bonds of the polymer backbone to rupture. This thermal scission produces volatile organic compounds and shorter chain oligomers that migrate to the surface of the melt. The accumulation of these molecules leads to splay marks on the surface of the molded part and can corrode the steel mold cavities over time.
Furthermore, the molecular weight distribution of the resin shifts downward, causing a significant reduction in impact resistance.
Analytical Detection
Gas chromatography combined with mass spectrometry allows for the identification of these volatile fragments. This laboratory test reveals the specific chemical structure of the degradation products to determine if they originate from the primary resin or from additives like flame retardants. It is a critical quality control step when evaluating regrind material for reuse.
Risk Mitigation
Reducing the residence time of the polymer melt in the injection cylinder prevents the buildup of degradative fragments. Molders must also control the drying process to eliminate moisture before processing hydrolytically sensitive resins like polycarbonate or polyamide. Dry resin prevents the hydrolysis that generates these unwanted breakdown molecules.