Meaning
Material failure characterized by rapid crack propagation with little to no plastic deformation prior to the break. Most polymers exhibit brittle fracture when subjected to high strain rates or temperatures below the glass transition point. This mode of failure results in a clean, sharp surface rather than the whitening or stretching seen in ductile breaks.
Energy Release
Rapid energy release occurs during the failure event because the polymer chains cannot reorient fast enough to absorb the impact. If a molded part experiences brittle fracture, the cause often relates to excessive molded-in stress or high levels of regrind. Reducing the cooling rate in the mold helps minimize the risk by allowing for more uniform shrinkage.
Thick wall sections also contribute to the problem by creating uneven thermal gradients during the solidification phase.
Fracture Prediction
Izod or Charpy impact tests provide the numerical data required to predict brittle fracture under load. The transition from ductile to brittle fracture happens at a specific temperature known as the DBTT. Engineers use these values to select resins for low-temperature applications where mechanical toughness is mandatory.
Ductility Transition
Frequent field failures lead to high warranty costs and potential liability issues. Selecting a resin with a higher elongation at break can mitigate the risk of brittle fracture in the final product. Even a small increase in rubber content in a blend alters how the part handles sudden loads.