Meaning
Internal reflection spectroscopy measures the infrared absorption spectrum of an optical interface to characterize chemical bonding within the outermost micrometers of a solid specimen. In plastics testing, atr-ftir spectrometry identifies base polymers alongside oxidation products without requiring destructive solvent dissolution or microtoming. The measurement governs chemical functional group identification at the immediate contact boundary, stopping where evanescent wave energy decays below detectable absorption thresholds.
Penetration Depth
Evanescent wave attenuation limits sampling to depths typically between half a micrometer and two micrometers into the resin matrix. High refractive index crystals such as germanium or diamond dictate the precise penetration profile across different infrared wavenumbers. Because atr-ftir spectrometry samples only this shallow skin, bulk core properties of thick injection moulded parts remain undetected.
Surface roughness or poor contact pressure diminishes spectral quality by introducing air gaps.
Surface Degradation
Photo-oxidation and thermal breakdown generate distinct carbonyl and hydroxyl absorption bands along the exposed faces of weathered components. When weathering degrades outdoor polyolefin mouldings, atr-ftir spectrometry tracks the increase in carbonyl index to verify stabilization failure. Regrind lots containing oxidized surface crusts yield higher carbonyl peaks that distinguish them from virgin feedstocks.
Processors use these spectral signatures to reject incoming recycled resin containing excessive oxidative decay before compounding begins.
Additive Quantification
Migratory processing aids and internal lubricants concentrate at the part surface, producing localized absorption signatures distinct from the bulk resin matrix. Calibration curves correlating absorbance band height to standard concentrations allow atr-ftir spectrometry to monitor bloom levels on blown films and injection moulded automotive trim. Insufficient additive migration causes mold release sticking or scuffing, whereas excessive migration produces hazing and bonding failures during printing or ultrasonic welding operations.
Reliable quantification requires consistent clamp pressure against the crystal face to avoid peak distortion from localized compliance differences across elastomeric or rigid samples. Tool surface finish directly influences how evenly the additive deposits against the analytical crystal during automated quality checks.