Meaning
Thermal or mechanical fragmentation of long chain saturated hydrocarbon polymers into shorter fragments results in a loss of viscosity and tack. During intensive mixing or extrusion, polyisobutene breakdown occurs when the polymer chains are subjected to high shear forces.
Shear Response
Mechanical energy input during processing can snap the molecular bonds of high molecular weight grades. If polyisobutene breakdown is excessive, the resulting low viscosity liquid will bleed out of the compound or fail to provide the necessary film strength. Processors must balance the need for thorough mixing with the risk of destroying the polymer structure.
Thermal Stability
High temperatures in the presence of oxygen accelerate the cleavage of the hydrocarbon backbone. Preventing polyisobutene breakdown requires the use of nitrogen blankets or effective antioxidant packages during the compounding stage. Monitoring the colour and smell of the melt can provide early warning signs of oxidative damage.
Quality Control
Testing for the extent of the degradation involves measuring the Mooney viscosity or the molecular weight distribution. A significant shift toward smaller molecules confirms that polyisobutene breakdown has taken place. Maintaining strict temperature limits and minimizing residence time in the extruder are the primary methods for preserving the integrity of the resin.