Meaning
Unintended leakage of molten polymer from the injection unit during the cooling phase or mold open time creates waste and potential safety hazards. Nozzle drool typically results from excessive melt temperature or inadequate screw decompression after the plasticizing stroke. This material can solidify on the mold face, preventing the tool from closing properly or damaging the parting line.
Thermal Imbalance
High heat at the tip of the injection unit reduces the viscosity of the resin. When nozzle drool persists, lowering the temperature of the front zone or the nozzle heater often solves the issue.
Decompression Failure
Suck-back settings pull the screw away from the melt to relieve the residual pressure. If nozzle drool continues despite a temperature reduction, the decompression distance may be too short to break the flow. Increasing this distance creates a small air gap that holds the melt back.
Careful adjustment prevents the introduction of air bubbles into the next shot.
Obstruction Risk
Cold slugs formed by leaking material can block the gate in the subsequent cycle. Because nozzle drool interferes with the consistency of the shot volume, it leads to weight fluctuations in the finished parts. Maintaining a clean nozzle interface ensures a reliable seal against the sprue bushing.