Meaning
Gas release defines the escape of carbon dioxide from a polymer melt or additive slurry during processing. This reaction occurs when carbonate additives decompose under high thermal or shear stress. Processors monitor carbon dioxide volatilization to avoid gas entrapment, which compromises both the look and the structure of moulded parts.
The rate of gas escape depends directly on the melt temperature and the pressure inside the extruder barrel.
Degradation Pathway
Thermal breakdown of carbonate salts occurs when the processing temperature exceeds the stability threshold of the mineral. This decomposition triggers carbon dioxide volatilization within the extruder barrel, creating pockets of gas in the melt. If the extruder does not have a vacuum venting system, this gas travels to the die and remains trapped in the finished compound.
Maintaining a processing temperature below the salt’s breakdown point prevents this early degradation.
Melt Stability
Entrained gas bubbles alter the viscosity and flow behavior of the molten plastic during moulding. When carbon dioxide volatilization occurs, the gas acts as a foaming agent, reducing the shear heating but also causing surge flow at the die. This fluctuation can lead to inconsistent wall thickness and uneven cooling across the part.
Solid fillers like calcium carbonate must be chosen for their thermal stability at the specific moulding temperature of the resin.
Part Defect
Surface splay and microscopic voids represent the main visual and mechanical issues caused by trapped gas. When the molten plastic enters the mould cavity, the trapped gas stretches along the part surface, creating silver streaks that are highly visible on dark or polished parts. This cosmetic issue is accompanied by a reduction in impact strength, as each micro-void acts as a stress concentrator that can initiate a crack when the part is dropped.
For this reason, moulders must measure the ash content and moisture of filled resin before starting a run, ensuring that any potential for carbon dioxide volatilization is eliminated before it can spoil a production batch. The loss of a single batch of parts can offset the cost savings of using cheaper fillers, making process control a priority.