Meaning
Material degradation processes that cause a thermoplastic to lose its impact strength and ductility when exposed to freezing temperatures result in brittle failures. Subzero embrittlement occurs when the temperature drops below the glass transition temperature of the polymer, immobilising the molecular chains. This transition prevents the polymer from absorbing energy through deformation.
Chain Immobilization
At these low temperatures, the cooperative movement of the polymer chain segments ceases, making the material behave like a rigid, glassy solid. When an impact occurs, the polymer cannot deform or dissipate the energy, which causes cracks to propagate rapidly through the material. This behaviour is especially common in semi-crystalline polymers like polypropylene, which have a glass transition temperature close to zero degrees Celsius.
Engineers must evaluate this property when designing parts for outdoor applications, such as automotive bumpers or storage crates.
Modifier Addition
To prevent this failure, compounders add impact modifiers or copolymerize the resin with elastomers that have a much lower glass transition temperature. These additives remain flexible at low temperatures, absorbing the impact energy and stopping cracks from growing. For example, adding ethylene-propylene rubber to polypropylene significantly reduces the brittle-to-ductile transition temperature.
This modification allows the moulded parts to survive impact even in freezing environments.
Ductile Transition
Laboratory tests measure this resistance by performing Izod or Charpy impact tests on specimens that have been conditioned in a subzero chamber. The tests are conducted at various low temperatures to find the point where the failure mode changes from ductile to brittle. This testing ensures that the selected resin meets the temperature requirements of the end product.