Meaning
Processing stabilizers undergo a chemical change as they neutralize hydroperoxides during the melting and extrusion of thermoplastics. Within a polyolefin matrix, oxidized irgafos 168 is the byproduct formed when the phosphite stabilizer reacts with oxygen-rich molecules. This conversion indicates that the additive has protected the polymer chains from thermal degradation.
Secondary antioxidants in the phosphite family rely on this mechanism to maintain material properties during high-temperature processing.
Stabilizer Efficiency
The ratio of active phosphite to the oxidized form reveals the extent of the heat history the material has endured. If a high level of oxidized irgafos 168 is present in virgin pellets, it suggests poor handling or excessive temperatures during the initial pelletizing step. Moulders use this information to adjust their own process settings to prevent further chain scission.
Degradation Product
Unlike the parent molecule, the oxidized version no longer provides protection against subsequent thermal events. It remains in the polymer as an inert species under most conditions.
Chemical Transformation
The reaction involves the addition of an oxygen atom to the phosphorus center of the molecule. This change is permanent and cannot be reversed by adding more virgin material to a regrind mix. If the concentration of the oxidized species becomes too high, it can affect the clarity or color of the final moulded part.